Hear the bits are S-7 and S-6.( Great hot cuts.)
The pins are like 4140.
(Great hammer heads.)
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
From: <PlumDon at aol.com>
To: <theforge at mailman.qth.net>
Sent: Thursday, July 15, 2004 11:23 AM
Subject: [TheForge] Jackhammer bits
> While in the process of scrapping out this week I came across a couple
> hundred pounds of 1" to 1-1/4" jack hammer bits. Could anyone tell me what
steel
> they are probably shaped from? I will offer them up at some upcoming
affiliate
> meets but would like to forge and temper one first.
>
> Also found quite a few 2" x 6" track pins from a bulldozer. Any ideas what
> that alloy might be?
>
> Kindest thanks for any advice.
>
> Don Plummer
> Plummer Design Works
> 392 Hallman Mill Road
> Phoenixville, PA 19460
> 610-495-5058
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list