Yall, try Cleveland Mica, Lakewood, OH.  Bruce Woodward gets his there,
a 36" square sheet was about $ 36.00 4 years ago, comes in many colors.
The sheets are composed of lots of smaller pieces held together with
shellac.  Apparently the stuff won't hold up in exterior applications.



 Stephen McGehee