Hi Andy,
Thanks for posting that. I am not sure what kind of smithing to call
it. It was fused in a electric kiln, hot forged in a propane forge
with a Kick Ass power hammer and 25# LG, then hot swedged, rolled in
a rolling mill , drawn through a draw plate, carved with a die
grinder, rolled some more, cut with a jewelers saw, gold brazed ,
turned on a lathe brazed again and finally polished. So I think I hit
almost all the techniques except casting :-)