[TheForge] And now for something very cool

Andy Vida [email protected]
Wed Jan 21 17:11:01 2004


Here's a little something by Jim Binnion.  It is a mokume mix of 22K
gold and pure iron.  Very warm combination.  Very nice.

	http://netlabs.net/~osan/Photos/22kFE.jpg

Not precisely blacksmithing, but close enough.

	-Andy