No..The East Coast Junk Yard hammer (EC-JYH) by Jock Dempsey used a disk-brake
for a clutch.
The North Carolina hammer used just a tire and steel wheel. The NC-JYH was
built by Steve Barringer of B2 Design, Ltd.
Daniel Kretchmar
www.irontreeworks.com
Isn't sanity really just a one trick pony, anyway? I mean, all you get is one
trick, rational thinking! But when you're good and crazy�ooh hoo hoo hoo�the
sky's the limit!
The Tick
Quoting Andy Vida <[email protected]>:
>
>
> Daniel Kretchmar wrote:
> >
> > Bob,
> > I built my own version of a NC-JYH power hammer from anvilfire.
>
> I remreber seeing that contraption at the 98 conference.
> I thought that was one of the most ingenious uses of junk
> that I have ever seen in my life. And it seemed to work very
> well. Using a disk brake as the clutch was brilliant.
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________