[TheForge] Microwaving Metals From the Virtual Junkyard

Chuck Robinson [email protected]
Tue Jan 6 10:28:00 2004


Check out  http://home.c2i.net/metaphor/mvpage.html
 "An insulating, but microwave transparent, ceramic fiber block is placed
around the cup area of the mould".
Chuck

----- Original Message -----
From: "Andy Vida" <[email protected]>
To: <[email protected]>
Sent: Monday, January 05, 2004 10:54 PM
Subject: Re: [TheForge] Microwaving Metals From the Virtual Junkyard


>
>
> James Binnion wrote:
>
> > The biggest
> > problem is getting rid of the radiant heat given off by the crucible
> > so that the oven doesn't melt or catch fire.
>
> I was wondering about this.  I can't see the oven in my
> kitchen surviving a 1 oz. melt without burning a hole through
> its bottom.
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>