[TheForge] tips for cleaning steel?

fonde taylor [email protected]
Mon Jan 5 18:10:35 2004


Great info.....thanks a ton!
fonde




--- [email protected] wrote:
> 
> OR  get several
> gallons of white vinegar.
> We used to use white wine vinegar for making a rust
> fit on worn machine 
> parts. There are differences between the white
> vinegars as to what acid they 
> contain. White wine vinegar has muratic acid, and
> will rust steel within minuets. 
> Just a cautionary note.
> Mikey
> 
> 
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post
> was in HTML
> or had an attachment.  Attachments are not allowed. 
> To learn how
> to post in Plain-Text go to:
> http://www.expita.com/nomime.html  ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
> 


__________________________________
Do you Yahoo!?
Find out what made the Top Yahoo! Searches of 2003
http://search.yahoo.com/top2003