There are well known aluminum solders, which you can order over the net. The=
=20
following is supposed to be able to do many different alloys:
Divesco Inc., PO Box 18097 4804 Cricklewood Ln., Charlotte, NC 28218  Tell:=20=
1=20
(704) 567-9800 or Tell: 1 (801) 705-3460 or Tell: 1 (877) 355-5641 Website:=20
http://divescoinc.com/   A-Lum-Rite (fluxless solderingproduct). Its melting=
=20
range is 715=BA F- 730=BA F, with a tensile strength of 47,000 PSI. Solders=20=
aluminum=20
and many other alloys.=20
Good Luck, and let us know how you come out.