[TheForge] forged leg hold trap

Ralph [email protected]
Sun Jan 4 02:22:06 2004


At 12:38 AM 1/4/04 -0600, you wrote:
>I recently bought a leg hold trap at an auction to use as an example for
>forging a trap.I made one and it was a pretty neat forging exercise. You
>have to draw out and punch spring steel, rivet pieces, form the trigger and
>get it all to fit and work as intended.
>  Has anyone else forged a trap or know someone who does?
>Please note that I dont intend for the trap to be used, but the forging
>respects what smiths were called upon to do in the past. It should be of
>interest to rendezvousers(sp.?) or history buffs.
>Bob

Have not completed one, but we at Fort Vancouver have several folks who 
have finished them. Why?

Ralph


"Good is the enemy of Excellent. Talent is not necessary for Excellence.
Persistence is necessary for Excellence. And Persistence is a Decision."