[TheForge] Microwaving Metals From the Virtual Junkyard

Carl Tappan [email protected]
Sat Jan 3 08:01:01 2004


That sounds like an excellent way to melt metal if it works, or an
excellent way to hurt yourself/burn down your shop if it doesn't. If
anyone trys this I would be very interested to know if it works as well
as claimed.
Carl Tappan

On Fri, 2004-01-02 at 22:31, Rob Fertner wrote:
> Over on keenjunk.com this was posted. It sounded so interesting I just had
> to share with the rest of you.
> 
> Copied from the Virtual Junkyard:
> Friend of mine sent me this thought y'all might enjoy it
> ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~+++
> Subject: [hobbicast] Microwave Melting Update
> 
> 
> Some of you may know that I make a living by developing new products
> and
> processes for the metal casting and steel making industries. About 6
> months ago,
> we started looking seriously at using microwave energy for melting
> metals.
> About $40,000 later, we have done an immense amount of lab work. We
> have
> successfully melted Aluminum, Bronze, Iron, Steel and even Glass in a
> simple 1000 watt
> microwave oven. The key points in doing this are as follows.
> 
> 1. You need do have either a special crucible that absorbs microwaves,
> or,
> you will need to have microwave absorbing materials nearby to a
> microwave
> transparent crucible.
> 
> So far, we have made all of our own crucibles. I can't tell you what we
> are
> using, because we fully intend to offer these crucibles for sale to the
> public,
> sometime this year. What I can tell you is that Silica (fused silica)
> is
> microwave transparent. Alumina becomes a microwave absorber at elevated
> temperatures. Once you get it hot, it will get very hot, very quickly
> in microwave
> energy. We have developed a mixture of refractories that can be shaped
> into a
> crucible that will reach over 2,000°F. in less than 5 minutes of
> microwave heating.
> 
> 2. You will need to use some fairly fancy refractory insulation to keep
> from
> burning up the inside of the microwave. We use a very low density solid
> or
> fibrous material that is about 70% Alumina and 30% Silica. You can
> either build a
> box and then put the crucible inside of it, or, you can line the whole
> inside
> of the microwave. Just remember that the radiant heat from a glowing
> crucible
> needs to be contained, or you will quickly burn the inside of the oven.
> Remove any plastic covers inside the microwave, or they will melt.
> 
> 3. You really need to keep close tabs on the temperature of the metal
> in
> order to avoid some serious over heating disasters. Last month, we over
> heated
> some Iron, which then melted through an Alumina crucible (that takes
> 3700°F), and
> then we vaporized the Iron (that takes about 5000°F). Things can get
> really
> hot really fast. Be prepared to shut down the power if you get into
> runaway
> heating. Have some really well insulated gloves or tongs to handle the
> crucible.
> 
> 4. Now, here's the neat part. We know that metals behave as microwave
> reflectors. They won't heat up in a microwave. BUT, we have learned
> that all metals
> will become microwave absorbers at elevated temperatures. We suspect
> that the
> temperature at which this occurs is about half of the melting point of
> the
> metal. We will know what the exact temperatures are later in January.
> 
> Once you reach this magical temperature, the metals will absorb the
> microwaves and you can melt lickety split! Virtually all of the energy
> that you put
> into the oven is going directly into the metal and causing molecular
> vibration
> (heating).
> 
> DON'T DO ANY OF THIS KIND OF STUFF IN YOUR WIFE'S MICROWAVE!
> 
> I have toasted 3 microwaves in the past 3 months, mainly because they
> got too
> hot from runaway heating. I melted through the bottom of one and the
> Iron ran
> out onto the table, along with a fair amount of microwave energy, which
> can
> be quite dangerous. If you are serious about doing this, you need to
> constantly
> measure for microwave leakage from the unit.
> 
> I expect to make a public announcement about the availability of these
> special crucibles and the refractory insulation for holding them,
> sometime in the
> next 3 months. This is no BS. We are quite serious about designing a
> microwave
> that will have the capability of melting at least one ton per hour, by
> the end
> of 2004. The eventual goal is to design and build a system that can
> melt
> several hundred tons a day.
> 
> I will keep all of my Hobbicast friends posted on our progress.
> 
> Tom Cobett
> Cleveland, OH
> 
> "In Pyro Veritas"
> 
> 
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
> 
> 
>