[TheForge] propane forge burner book

H and P Foster [email protected]
Sun Feb 29 10:27:07 2004


 Bill

Your description of two combination forced air and atmospheric air burners
might be understandable to some, but not to me.  I thought one used either
atmospheric or blown.  Is it set up that way so you can still forge when the
power is out?  Would love to learn more, perhaps a couple of photos,
drawings etc.  I'm always interested in new forge designs.

Harry 
Rusty Dog Forge

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Bill & Kirsten
Sent: Sunday, February 29, 2004 9:05 AM
To: [email protected]
Subject: Re: [TheForge] propane forge burner book

My forge is nothing new.  I have been using it for about 15 years now.  It
is a barrel forge 24" long on its side with two combination forced air and
atmospheric air burners.  The barrel is lined with B density FiberFrax as a
liner and castable on the floor to catch the flux.  I use a sheet of wax
paper to separate the liner from the castable when I am placing the castible
on top of the liner in the bottom of the forge.  This allows me to change
the castable, when it gets bad, without damaging the liner.
The forge maintains a temperature of around 2800 F which is great for my
Damascus.  I weld on the average of 4 to 5 hrs. each day.
Bill
[email protected]
 http://home.centurytel.net/Fiorini_and_Skiles

----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Saturday, February 28, 2004 9:46 PM
Subject: Re: [TheForge] propane forge burner book


> In a message dated 2/28/2004 5:33:40 AM Pacific Standard Time, 
> [email protected] writes:
> I have found that the color coded n. valve from Grainger works the 
> best
for
> me.  It has great control.
> Bill
> Thanks for the update, Bill. Why don't you tell us a little bit about 
> your forge and what it's like working with it?
> Mikey
>
>
> --- StripMime Report -- processed MIME parts --- multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post was in HTML or 
> had an attachment.  Attachments are not allowed.  To learn how to post 
> in Plain-Text go to: http://www.expita.com/nomime.html  --- 
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>

_______________________________________________