Try Fazios down by Swedesboro. Don't have their # handy. "Mark A. Pesetsky" wrote: > > I used 4" x 4" 4340 un hardened for my Kinyon style hammer and > after years of almost daily use, they show very little wear. > http://magichammer.freeservers.com > > dave m > > I will have to see if I can track some of this material down locally. If > not, is there a place online that you know of that supplies this material?