A blade may also be brought back into alignment by putting in into a vice 
with 3 rounds rods
2 on one side and on on the other.I have a set of slip on jaws for the vise 
with one side having the rods welded to the outside edges and the other has one 
rod in the middle
:< looking down from the top you would be looking at the ends of the rods.It 
works vey well to straighten blades
Bob