Mike,
Sorry, misunderstood. I'll try that tonight. I had given up on them and
was going to toss them. I figured that if I hit it again, I would have to
regrind them and I really didn't want to do that.
Dan
www.irontreeworks.com
"Isn't sanity really just a one trick pony, anyway? I mean, all you get is one
trick, rational thinking! But when you're good and crazy…ooh hoo hoo hoo…the
sky's the limit!"
The Tick
Quoting Mike McKim <[email protected]>:
> I was referring to recovering a previously warped blade.
>
>
>
>
> > Mike,
> > Unfortunatley, that would require that I know which way it is going to
> warp
> > before the quench.
> >
> > I think the normalizing idea sounds the most reasonable. I'll try that
> next
> > time.
> >
> > Danr Katlasmiğr
> > www.irontreeworks.com
> >
> > "Isn't sanity really just a one trick pony, anyway? I mean, all you get is
> one
> > trick, rational thinking! But when you're good and crazy.ooh hoo hoo
> hoo.the
> > sky's the limit!"
> > The Tick
> >
> >
> > Quoting Mike McKim <[email protected]>:
> >
> > > Can it be manually warped in the opposite direction in an equal degree
> while
> > > hot. Upon quenching in water the cooling induced warp would cancel out?
> > >
> > >
> > > > ****This is where it warps*****
> > > > 4. Harden (heat to orange and quench in water)
> > > > ****This is where it warps*****
> > >
> > > _______________________________________________
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login: [email protected]
> > > password: anvil
> > > ___________
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________