I put some on my forge and like it real well.
Worked best when brushed on the Kaowool/durablanket lining.
I think Larry has Plistix for sale now, but you'll have to ask him..
Andy G.

> 
> Larry Zoeller wrote:
> 
> >To all,
> >I have been working with my local refractory supplier to find a possible
> >replacement or substitute for ITC 100.  They have recommended 
> Plistix 900F,
> >the price would be about a third of the cost of ITC 100....
> >
> I am building three Sandia forges from the  ABANA plans. I haven't been 
> able to find
> Plistix . I have a pint of ITC-100 and I will need to get more 
> refractory. So...Do you recommend
> the other?
> Thank you.
> Kenny O
> 
> 
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment.  Attachments are not allowed.  To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html  ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
>