The November/December 2004 issue of The Home Shop Machinist has an
article about superquench. He states that he uses a quarter cup of
Cascade liquid dishwasher detergent in 2 gallons of tap water and that
it works as well as the original recipe.
Rob
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Andrew Vida
Sent: Tuesday, December 28, 2004 12:24 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] superquench questions
Schade wrote:
>
> I bought a set of the dovetail die adaptors for my LG 25 from Sid. I
> have some chunks of 2"x3" to make a few sets of dies.
>
> Do any of you use "superquench" on hammer dies?
I think a hammer die might be a bit large, but what the hell, it
can't
hurt to try.
>
> What is the current recipe?
5 gal water
5# table salt (wonder if epsom salts would do)
26Oz Blue Dawn detergent
7 Oz Jetdry or similar surfactant.
>
> Is there somewhere online to get the Shaklee stuff?
Don't need it. Jetdry works. Probably the same stuff.
>
> Has anyone ever Rockwelled after superquenching?
>
> Should I weld the die together before superquenching?
>
> Is a 5 gallon bucket of SQ big enuf to quench hammer dies?
>
> Thanks.
>
> Bob
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list