Hot bluing with various nitrate mixtures (sodium nitrate, pottassium nitrate). The cold bluing has a rotten egg smell, so I am guessing some sort of sulphuric acid? Charles Bruce Freeman wrote: >Gun blue?! What IS it? Do you want to eat off it? > > >