[TheForge] Re: Powder Damascus
Andrew Vida
osan at netlabs.net
Sat Dec 11 11:26:39 EST 2004
Dan Scheid wrote:
>
> Can you use a power hammer instead of the press or must it be "pressed"
> Dan Scheid
Press is going to give much better control and a better guarantee
against shearing the welds, all 250 million of them, when trying to
stick the billet. Initial sticking in a stack is a comparatively
delicate matter. Light pressure and no violence seems to work best.