[TheForge] Re: Powder Damascus
Mike Spencer
mspencer at tallships.ca
Fri Dec 10 01:24:40 EST 2004
> UMBA library has a couple of demos of powder damascus one by Peter
> Martin and the other by Jim Batson.
I'll be dippt. Guess I haven't been paying attention.
> Most use thin nickel sheet as the powder separator although Jim said
> just standard paper card stock would work it just leaves a fuzzier line
> between the two types of steel due to carbon migration.
> Both used super glue to make the pattern for the design
I don't quite get that. Guess I'm going to have to get somebody to
explain the details to me or get the videos.
Thanks for the enlightenment.
- Mike
--
Michael Spencer Nova Scotia, Canada .~.
/V\
mspencer at tallships.ca /( )\
http://home.tallships.ca/mspencer/ ^^-^^
--
More information about the TheForge
mailing list