For more brazing information than most of us could ever use refer to
http://www.handyharmancanada.com/TheBrazingBook/bbook.htm
A side note on the silfoss and its variants; it is mostly intended to be
used for fluxless joining of copper tubing. It will work on many other
metals when used with a flux, but is primarily intended for fluxless joining
of copper.The joints that it produces are very hard and therefore brittle.
It has a very low silver content, which maxes out at a 15% BCuP alloy.
For joining ferrous metals and copper alloys(brasses and bronzes) try a
'silver solder' BAg alloy, typically 45% silver. The BAg alloys must all be
used with a flux regardless of the parent metals.
Please refer to the following chart
http://www.handyharmancanada.com/TheBrazingBook/Section%203/Part%209.htm#Bra
zing%20Filler%20Metals%20Based
Paul C. Sperbeck
My Grandfather was a blacksmith,
and It didn't do me one damn bit of good...
The information in this transmission is intended to be totally worthless
and devoid of any benefit to anyone with the exception of, possibly, the
intended recipient. If you received this communication in error or if you
accidentally read it when it wasn't addressed to you, then please
immediately delete all of your saved game files, mp3s and email addresses
and then energetically beat yourself about the head and shoulders with a
recent technology publication of your choice. All other more intelligent
actions taken in response to this information are prohibited, so there.
The following added for automatic email harvesters!
abuse at worldatt.net abuse at prodigy.net abuse at bellsouth.net abuse at yahoo.com
UCE at FTC.GOV abuse at tesco.net abuse at freeserve.net
---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.744 / Virus Database: 496 - Release Date: 8/24/2004
More information about the TheForge
mailing list