>find is a place in Portland OR. that would make me one for about $500.00.
>So out to the shop. I built the inside of the hub up with 7018 doing a
>narrow weave pass, let cool, chip slag, rotate a new area to the bottom and
>repeat until I had enough metal build up. ...<smpi>...
>It took about two hours but it worked and the field is roto tilled.
>Darrell