[TheForge] air hammer timing

kim george klgeorge at kent.edu
Sun Aug 22 10:05:39 EDT 2004


The hammer is together but I'm only getting a 3" stroke . The four way is 
cycling fast. The only thing I can think of is the 2" cylinder takes enough 
air compared to the 1 1/2" cylinder to throw the timing off. Would a needle 
valve on the 1/8" air line slow things down enough to get a full stroke?

Kim George