[TheForge] Green Copper

GHS ghs at execpc.com
Thu Aug 19 09:23:21 EDT 2004


Free sulfur in almost any form will speed the process.
They will oxidize, turn brown, almost immediately. The green is a slower 
process if left to nature. It used to be quick when everyone burned coal.

Mike Graf

Frederick Faller wrote:

> A friend of mine just installed copper gutters and
> wants to know how to promote the green copper oxide.
> Is there a way to do this? (not interested in faux
> verdigris finishes, just wants to get the copper to
> oxidize green)
> 
> Frederick Faller
> 
> 
> =====
> Frederick W. Faller
> Shiloh Forge Ironware http://users.rcn.com/ffaller/SFI_web.htm
> www.immerland.com
> 
> 
> 		
> _______________________________
> Do you Yahoo!?
> Win 1 of 4,000 free domain names from Yahoo! Enter now.
> http://promotions.yahoo.com/goldrush
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 
> 
> _____________________________________________________
> This message scanned for viruses by CoreComm
> 
> 

-- 
  Please visit us at http://www.gaudeteforge.com/



More information about the TheForge mailing list