[TheForge] More gas conversion questions
Jerry Frost
frosty at customcpu.com
Sun Aug 15 13:30:04 EDT 2004
----- Original Message -----
From: "TOOL GYPSY" <toolgypsy at hotmail.com>
To: <theforge at mailman.qth.net>
Sent: Sunday, August 15, 2004 5:35 AM
Subject: [TheForge] More gas conversion questions
> Good morning all
> I have an old small gas furnace that was used to heat soldering
> irons.Can this be converted to propane to use as a small forge or is this
> just wishfull thinking?
> Paddy P the wannabe
>
It'll probably cost more and be more hassle to convert it than building a
forge. However, it might, just MIGHT make a decent annealing oven with a
little mod.
Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
More information about the TheForge