[TheForge] air hammer &damascus?

kim george klgeorge at kent.edu
Sat Aug 14 11:52:19 EDT 2004


Since with a little luck my air hammer will be up and running next week.It 
should be time to think of some tooling. I want to make a spring fuller to 
do some rain drop patterns.How thick should the billet be and how deep of a 
depression should be made? I do mostly flat grinds and don't want to grind 
the pattern out.