[TheForge] Gas forge, with pictures :^)

Mark A. Pesetsky pesetsky at Princeton.EDU
Sun Aug 8 08:48:43 EDT 2004



> 
> Hullo all,
> 
> I finally have gotten the forge to the testable stage. Many thanks 
> to 
> Dave Lisch for hosting the blacksmithing swapmeet last weekend, 
> without 
> that having happened, it would have taken me a good deal longer to 
> acheive this.  Woo. :^)
> 
> This is very much still in the testing phase, and I still need to 
> make 
> the stand (and get a shop :D), but it's getting closer.
> 
> Pictures:  http://www.dreamingcrow.com/gabriel/gallery/forging
> 


Nice work...

Might want to consider coating the insulation with some kind of refractory. Breathing the fibers from the INSAWOOL typ material is quite harmful.