[TheForge] titanium
Hochewa at aol.com
Hochewa at aol.com
Sat Aug 7 22:20:27 EDT 2004
To All,
CP (commercially pure) titanium does not harden except through cold work.
Just clean off the oxide after forging and use a sharp edge on the flint. It
takes a lot more effort than does steel but the spark is awesome.
Hochewa
In a message dated 8/7/2004 5:05:22 PM Eastern Standard Time,
kc7pme at tscnet.com writes:
Do you use the Titanium striker "as forged"? Do you quench in water like HC
steel or do any heat treatment?
Jeff