[TheForge] titanium
The Wilson's
kc7pme at tscnet.com
Sat Aug 7 17:02:03 EDT 2004
Do you use the Titanium striker "as forged"? Do you quench in water like HC
steel or do any heat treatment?
Jeff
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Hochewa at aol.com
Sent: Wednesday, July 28, 2004 5:20 PM
To: theforge at mailman.qth.net
Subject: Re: [TheForge] titanium
To All,
I use CP. No wories about alloy content. Just forge and strike really hard
with a sharp flint.
Hochewa
In a message dated 7/28/2004 2:53:58 PM Eastern Standard Time,
osan at netlabs.net writes:
> Mark Williams wrote:
> >
> >Titanium makes great strikers for a "Flint &Steel" set.
>
> CP or alloy?
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list