I use half-inch round hot-rolled mild steel. 3/8 square does a good job,
too. I made one out of a spring, and it sounded real good, but
straightening out a coil spring just wasn't worth it.
Mike Murphy
-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Woolley
Sent: Friday, April 30, 2004 7:09 PM
To: [email protected]
Subject: Re: [TheForge] Triangles
What kind of steel do you use to make your triangles?
Michael H. Murphy wrote:
>I make one with four sides. There is an eye punched in the corner opposite
>to the open corner, which has a string through it to hang the four-sided
>triangle(I call 'em dinner bells) from. Regular three-sided dinner bells
>should have the opening on one of the bottom corners. I've tried it both
>ways, and it works better that way.
>
>Mike Murphy
>
>-----Original Message-----
>From: [email protected]
[mailto:[email protected]]
>On Behalf Of Rich Maynard
>Sent: Thursday, April 29, 2004 5:41 PM
>To: [email protected]
>Subject: RE: [TheForge] Triangles
>
>Good point. And with one being twice as long as the other, they should be
an
>octave apart.
>
>Rich M.
>
>
>
>>-----Original Message-----
>>From: [email protected]
>>[mailto:[email protected]]On Behalf Of Michael Horgan
>>Sent: 29 April 2004 23:35
>>To: [email protected]
>>Subject: Re: [TheForge] Triangles
>>
>>
>>Usually down in a corner. This gives you two different lengths of steel
>>ringing, making a pleasing chime tone. Try one both ways and listen, see
>>what you think.
>>
>>At 12:12 PM 4/29/2004, you wrote:
>>
>>
>>>Should the opening on a triangle that you ring be up next to the eye or
>>>down in one of the bottom corners?
>>>
>>>Keith "Sparky" Holmes
>>>
>>>
>>Michael D. Horgan , [email protected]
>>http://members.aol.com/lughaid/
>>posting from
>> A BRAZEN FORGERY
>>Blacksmithing and Metalwork
>>Claremont, Ca.
>>
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: [email protected]
>>password: anvil
>>___________
>>
>>
>>
>>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>
>
>
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed. To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html ---
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________