Jeff, Obviously a spring steel - Maybe 1084? Barking Crow wrote: > > Does anyone happen to know what type of steel the tines from a standard old > fashioned leaf rake are made of? Guesses? Maybe 1040? Just a guess. I'm not a leaf rake expert. :)