Andy Vida wrote:
> 
> Barking Crow wrote:
> >
> > Does anyone happen to know what type of steel the tines from a standard old
> > fashioned leaf rake are made of?  Guesses?
> 
>         Maybe 1040?  Just a guess.  I'm not a leaf rake expert. :)

Thinking it might be higher. The ones I have throw excellent sparks and
make good punches and fire starters.

Ralph
-- 




                                                        
					