The clamp I use only when I need to get a new or different purchase on 
the stock with my tongs.

The single hard blow I only have used in conjunction with a die that I 
wanted just one hard crushing blow to avoid getting a double strike mark.

Mike Graf

Jerry Frost wrote:

> Thanks Mike.
> 
> The poll now stands at 1 yea - 2 nae votes.
> 
> How often and for what do you use the clamp and or dead blow?
> 
> Frosty
> ------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
> 
> Meadow Lakes, AK.
> 
> 
> ----- Original Message ----- 
> From: "Michael Wolfe" <[email protected]>
> To: <[email protected]>
> Sent: Saturday, April 17, 2004 4:13 AM
> Subject: Re: [TheForge] Speaking of hammers
> 
> 
> 
>>YEA YEA 
>>Mike Wolfe
>>--- "David E. Smucker" <[email protected]>
>>wrote:
>>
>>>I have the clamp feature on my early "Bull Hammer"
>>>serial number 8, and
>>>never use it.  I fact depending on tooling height it
>>>is a not something you
>>>want to have happen.  Vote is now 0 to 2
>>>
>>>Dave Smucker
> 
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
> 
> 
> 
> _____________________________________________________
> This message scanned for viruses by CoreComm
> 
> 

-- 
  Please visit us at http://www.gaudeteforge.com/