>" Stoker coal heats the blacksmith more than the metal."
>
>As in, it burns upward ( to heat boiler tubes).
>
>dan tull
Yep, it sure does. That's the result of the relatively high content of
volatile matter (oils 'n stuff). That's one of the things that makes
Pocahontas so good, the heat is in the coke, not in the flame.
Dave Brown
Heritage Smithing