[TheForge] Trenton ID

Gladish Family [email protected]
Tue Apr 6 21:37:00 2004


Thanx for the tip- my MIG is pretty wimpy for a job like that, but Lincore
is all over the place, so will try it next time.
A. G.

 Every normal man must be tempted at times, to spit on his hands, hoist
the black flag, and begin slitting throats.
    -- H.L. Mencken.    1880-1956


> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of Andy Vida
> Sent: Tuesday, April 06, 2004 4:46 PM
> To: [email protected]
> Subject: Re: [TheForge] Trenton ID
>
>
>
>
> Gladish Family wrote:
> >
> > Steve-
> > If you find some, let me know- Central Welding is the only
> supplier in my
> > usual rambling distance and they've never heard of it.
> > I've used the Stoody and it held up fine but is difficult to
> run and tends
> > to be pitted- don't know why...might be operator error.  ;-)
>
> 	If you have MIG, Lincore 50 works VERY well.  Last spool I bought
> 	was $130.
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>