At 07:29 PM 9/27/2003 -0700, you wrote:

>Well, could be cast, use a sweep to make the simple sand molds.Pretty 
>heavy, though.  Could be done in one shot over a hollow die.Use an 
>annealed blank bolted to a die form. Draw a vacuum, then put at the bottom 
>of a tank, then set off an underwater explosion above it. The pressure 
>wave does a nice job of forming the blank to the die.  <grin> Your mileage 
>may vary.


         This is called hydro-forming.  Not something to be done in one's 
backyard.


---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.516 / Virus Database: 313 - Release Date: 9/1/2003


--- StripMime Report -- processed MIME parts ---
multipart/mixed
  text/plain (text body -- kept)
  text/plain (text body -- kept)
The reason this message is shown is because the post was in HTML
or had an attachment.  Attachments are not allowed.  To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html  ---