[TheForge] copper balls
Mike Linn
[email protected]
Sat Sep 27 22:31:00 2003
Buy them... its a lot quicker and safer...
http://www.globekit.com/catalogue.html
http://www.centurymetalspinning.com/products/
At 07:42 PM 9/27/2003, you wrote:
>Talked to a customer today who wants 2 copper balls for his patio 30"-36"
>in diameter. One will become a Bar-B-Q and the other an ice bucket.
>Has anyone had any experiance forming anything this big?
>All I can think of is raising which sounds like a ton of pounding or
>spinning on a setup similar to Mike Spencers air hammer power plant, big
>form and copper disc bolted to an axle. The latter sounds half scary and
>would also be quite a bit of work even before moving any copper.
>Any suggestions wil be appreciated.
>Randy Mundt
Mike Linn
Artist Blacksmith
McCalla, AL
AFC Webmaster
http://afc.abana-chapter.com
"The smallest minority on earth is the individual.
Those who deny individual rights cannot
claim to be defenders of minorities."
Ayn Rand