>   I second the use of scotchbrite.  I  used it for final finish on an AL 
> handrail.  It leaves fine lines but is nice.  A coating of Boeshield 
>  last  brings a nice oiled shine.

Yup, that was the stuff!
Got just the finish I wanted.