Fwd: [TheForge] Re: Welding SS

James Binnion [email protected]
Sat Sep 13 21:18:01 2003


Black Flux. There are several Mfr.  that make it (Harris and 
Handy&Harmon and probably others.) It is a Boron modified paste type 
brazing flux that will work much better on hard to braze materials like 
stainless. It has a deep brown almost black color.

Jim


On Saturday, September 13, 2003, at 07:09 AM, Lynn Emrich wrote:

> Back to welding SS. I tried to silver braze some 316C
> stainless with little success. I took the part to
> someone that is a much better welder than I and he had
> problems also. Is there a way to braze SS? If I
> promace not to tell will you give me the the secret?
> :)
> Thanks, Lynn
>