From: "Chuck Robinson" <[email protected]>
Subject: Re: [TheForge] Welding SS
> The easiest contrasting metal to add is Nickel foil; a little goes a long
> way.
> After folding the billet to about 80 layers, forge the billet to square,
> octagon then round.
> Twist it several turns then fold it again, weld, and forge into the shape
> you want.
> Very dramatic twisted contrasting layers.
> Chuck
>
>
I just spent a good 45 mins. digging through my change jugs and managed to
turn up 6 quarters and 3 dimes Canadian, didn't even make wages. <sigh>
Found a couple bucks of spendable US coinage though so tomorrow's coffee is
paid up anyway.
Do I need to use anything besides my 4 pts borax : 1 part boric acid for a
flux?
Thanks.