Great for a knife or many other  tools, but not so good for a fireplace
shovel that will be subjected to repeated heating and cooling. Stress crack
city.
Chuck
----- Original Message -----
From: "Dan Tull" <[email protected]>
To: <[email protected]>
Sent: Friday, September 12, 2003 8:53 AM
Subject: Re: [TheForge] Welding SS


> L6 saw blade etches silver. Has a bunch of chrome.Blue banding strapping
> seems to be 1095 and
> w/ L6 makes a nice pattern. Welds easy ,too.
>
>