There are a number of factors determining what your minimum operating psi.
will be for a naturally aspirated burner. You can't just look at the
pressure gage; you have to adjust your expectations to the entire device's
characteristics.

Thanks to your reasonably complete description I can hazard a couple
opinions with some hope of accuracy. <grin>

First, you have a 90* bend in the burner tube, this will cause back
pressure, requiring more psi to drive around.

Second, you're running a "sidearm" configuration jet ejector with only a 1
1/4" intake on a 1" tube. This is not a free breathing configuration and
requires higher psi to draw sufficient air.

Thirdly you're using a 0.035" orifice which requires more psi to deliver
sufficient propane. How well aligned is your jet in relation to the burner
tube? This is really critical.

You have several  options open:

First accept higher operating psi as normal for your burner, you're getting
plenty of heat even though it doesn't idle like you want. Still, running a
"smaller" orifice delivers less gas at a given psi so you may have the
economy you're looking for already. In short it could already be singing the
tune you want, just in a higher key. <grin>

Second look at changing the 90* to a longer sweep or even two 45*s . This
will increase the radius of the direction change and reduce the back
pressure a bit though probably not enough for a stable idle. You should also
place any bends as far as practical from the throat (narrowest point between
the intake and burner tube) of the burner. The longer the jet of propane can
travel down the exact (as possible) center of the tube, the more efficiently
it'll draw.

Thirdly you could try a "T" configuration jet ejector, I have a pic of mine
on photoaccess under forges and hoods. Mine is a 1 1/2" x 1 1/2" x 1 1/2"
"T" reduced to 1" with a simple bushing. I had to drill through the back of
the "T" to install the gas supply. (#7 drill, tapped 1/8" pipe) It has two 1
1/2" intake ports and runs with a 0.045" orifice (Miller mig tip). Mine
burns stably at any psi my gage registers, 30psi. to below 1 psi. but the
low end is inadequate to keep my forge in range so I just run it around 5
psi. My old forge only has 1" of Kaowool insulation around 3/4" rammable
refractory so if I idle it very low it cools down and I burn more fuel
reheating it than just keeping a steady burn. I do bump the psi up to 7-8
psi. to weld but for general forging 5 psi. is just right.

Fourth, filing the port in your forge liner to form a taper might be well
worthwhile. On my next forge I plan on building my burner nozzles into the
refractory liner myself, mostly to save on tube burnout but also to improve
performance.

Lastly, how completely are you closing your forge up? If you're not allowing
enough opening for exhaust gasses to escape you're really building back
pressure and inhibiting your burner performance.

Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.


----- Original Message -----
From: "Marc Godbout" <[email protected]>
To: "TheForge" <[email protected]>
Sent: Saturday, September 06, 2003 7:13 AM
Subject: [TheForge] Problems with propane burner


> First of all, my castable project went really well. The forge has been
> through its first firing with only a few small stress cracks. Now time
> will tell.
>
> But my new burner has some problems and I'm hoping to get some ideas
> from you guys. I'm trying some slightly different design to better match
> my application. First, the mixing tube is a 90 degree sweep of 1" rigid
> conduit. I wanted to lower the profile.
>
> The other difference is that I cast the nozzle into the refractory wall,
> but I didn't flare it. Also, this is a side-arm, using a 1 1/4" cross
> fitting with a reducer to the 1" tube. I've got a .035 mig tip for the
> orifice.
>
> The problem is that I have a tough time keeping it running at low
> pressures. I don't have a gauge on it, but from the sound it's probably
> well over 5 psi, maybe even 10, before it starts sputtering (with a
> nifty "whoop" sound), and then the flame travels all the way to the mig
> tip. I was able to get much lower when I had it out of the forge, using
> just a straight pipe for the nozzle.
>
> High end is no problem. Things get bright yellow hot in there in no time
> at all. And that's with just one burner in an 18" long half-tube,
> half-stacked-brick, with 25 psi (the max that my delivery system will
> do).
>
> I'd like to get really low for idling between heats to save propane, so
> any thoughts would be welcome. Should I try flaring the nozzle? This
> castable is easy enough to carve with a round rasp.
>
> Thanks.
>
> -Marc
>
> --
> Marc Godbout
> http://www.ironringforge.com
>
> New England Blacksmiths Membership Director
> http://www.newenglandblacksmiths.org
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>