[TheForge] Power hammer anvil
Dave Brown
[email protected]
Wed Oct 29 09:31:01 2003
Dan,
If you think your's walks, you should have seen my 50# LG dance before I
pinned it in place.
Do you have a rubber horse stall mat or something similar under it? It
will accentuate the tendency to walk.
Drill some holes through the base plate and then down into the concrete ...
make them about 1/2" diameter. Knock in rebar (or any 1/2" rnd steel bar)
pins through the plate and into the concrete. This won't eliminate all of
the rocking, but it won't walk.
Dave Brown
Green Bay, WI
At 22:39 10/28/03, you wrote:
>Hey All,
> My JYC power hammer is walking. I know why. The anvil ain't
>heavy enough. I used 6 inch square thick walled tube, .5 inches thick. I
>filled it with sand but that didn't work. Any ideas on how I can make it
>heavier?
>
>Could I cut off the die holder, fill it with melted lead and then reweld the
>die holder back on?
>
>suggestions?
>
>Daniel
>www.irontreeworks.com
>
>you can see a picture of it at http://www.irontreeworks.com/the_shop.htm