This sounds like Meagan Crowley's work
Larry Brown


>I did watch another demonstrator doing pipe/tube at the 2002 ABANA
>conference.  She made chain links out of round rod and rolled the pipe
>ends to capture the U bent rod making the link.  She also did some
>flower shapes collapsing the pipe in various places.  When I catch up a
>couple of other projects I should rewatch the tapes I shot.
>