[TheForge] outdoor finish for rusty steel

theron [email protected]
Tue Nov 25 00:33:00 2003


I am working on a sculpture that will be installed in a covered =
vestibule outside of a bank its in Charlotte NC=20
not in the direct sunlight and not in direct rain
I am thinking about using linseed oil and wax formula=20
with the explanation to the client that the piece will need routine =
maintenance=20
do any of you use oil and wax for outdoor rusted sculptures? if so how =
has it worked out for you .
what about incralac? has anyone had experience with this on steel =
outdoors?