[TheForge] Suggestions needed for scroungeable steel

Bruce Freeman [email protected]
Wed Nov 19 08:48:01 2003


Pete,
This particular TH will be quite simple.  The ram face IS the hammer
face.  No upper tooling.  Hence it needs to be hard enough not to
mushroom when it strikes a tool.  I expect to harden and temper it like
an ordinary hammer face.
Bruce
NJ

>>> [email protected] 11/18/2003 11:33:20 PM >>>

Bruce:
I'd respectfully argue that a hard face on a treadle hammer is not 
desirable. A softer face will "stick" to a struck tool allowing greater

latitude in alignment. With a hard face, more struck tools go flying to

mysterious locations where they hide for years.    Pete F

Bruce Freeman wrote:

>I'm designing another treadle hammer, a lightweight job.  I want the
ram
>to be 20#.  What would be ideal is square or roundstock of about 2
>sq.in. in cross-section (i.e., 2" square or 2.25" round) and about
18"
>long.  
> 
>Ideally, the material would be suitable for use as a hammer, with
>ordinary hardening & tempering.  Exotic materials not needed, but
mild
>steel wouldn't be appropriate unless faced with tool steel (a
>possibility I'd prefer to avoid).
> 
>Since I prefer to design in scroungeable materials, I could use some
>suggestions as to sources of such steel.  The truck axles I've seen
are
>of smaller diameter than this (though I've seen tractors with axles
of
>3" dia.).  Track pins seem to be shorter than this - like 8" or so. 
>Anyone have any other suggestions - preferably of materials you'd
have
>no particular trouble scrounging yourself?
> 
>Thanks in advance,
> 
>Bruce
>NJ
> 
> 
> 
> 
> 
>
>
>--- StripMime Report -- processed MIME parts ---
>multipart/alternative
>  text/plain (text body -- kept)
>  text/html
>The reason this message is shown is because the post was in HTML
>or had an attachment.  Attachments are not allowed.  To learn how
>to post in Plain-Text go to: http://www.expita.com/nomime.html  ---
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>
>
>
>  
>

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________





--- StripMime Report -- processed MIME parts ---
multipart/alternative
  text/plain (text body -- kept)
  text/html
The reason this message is shown is because the post was in HTML
or had an attachment.  Attachments are not allowed.  To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html  ---