Use auto wheel weights. You don't want to use pure lead as it is too
soft. Wheel weights have enough alloying elements to make good babbitt.
I used it in my triphammer on advice from a guy from New England
Blacksmiths.
Steve Smith
KEN O'OUGHLIN wrote:
> Ther was this fan housing which was being heated in the oven so that it could be treated with some Yellen's iron preserve stuff, I forgot about it and the babbitt melted out.
> I can't find a place that will sell less than 25# . Does someone know of a way to get 1 or 2# ?