> Moisture causes the milky laquer finish,

Now that I think about what went milky and what the conditions were when the
finish went on, it's plain to see that moisture got trapped.
Funny how the discoloration didn't show up immediately- though one item was
a wedding present, the rest were just things for around my house, so no
great harm done...