[TheForge] clear coat question

Gladish Family [email protected]
Mon May 26 15:58:01 2003


Sure wish I knew why spray lacquer sometimes goes milky and sometimes
doesn't.
I made a series of vessels finished with sray lacquer (I'm not talking about
acrylic "lacquer") that all look great after a year, but some other forged
peices have really unattractive white splotchiness.
Anybody got a clue?
Thanks,
Andy G.

 I don't need time. What I need is a deadline. -Duke Ellington

> > Lacquer is solvent based material with a high VOC content, and
> it "dries"
> > literally, the VOC evaporate leaving a deposited coating any simplex
> > materials that can be dissolved can be used to form lacquers..
>