[TheForge] Re: More air hammer pics up
Andrew Vida
[email protected]
Mon May 26 15:54:19 2003
Mike Spencer wrote:
> Andy> I was thinking if you would gun drill the crank with a small oil
> Andy> gallery and feed oil through the crank to the bearing, you would
> Andy> have a great oiling system.
>
> I hope not to take the crank out, at least not until I know it's going
> to work at all. Together with that big gear, it would be very
> awkward. The main crank bearings are lubed from oil tanks on either
> side. But I'm trying to figure out how to fix up an oil pump for the
> conrod bearings. The conrod is already bored in such a way as to make
> that doable. Still at the munbling & muttering stage.
I understand your reluctance. Then how about a flexible
hose from a tank to a fitting in the rod?
How is the big end bearing oiled now?