[TheForge] Little Giant frame repair
lama
[email protected]
Tue May 20 12:41:01 2003
Haven't had one come loose yet. It's steel to steel, I don't think that
bolting to cast iron would be any dif.
dave m
----- Original Message -----
From: "Larry and Pat Brown" <[email protected]>
To: <[email protected]>
Sent: Tuesday, May 20, 2003 4:22 AM
Subject: Re: [TheForge] Little Giant frame repair
>
> To the guys who made bolt on dies for your Kinyon style air hammers;
> Are there any problems with the bolts coming loose from the impact?
> Do you think a similar die bolted to cast iron would work also?
> Larry
>
>
>
> > As for drilling and tapping, could you elaborate? I'm not
> > sure I'm understanding, but if you're suggesting that the
> > block be bolted to the base of the hammer, I would not be
> > in favor of that solution, the impacts and vibrations being
> > what they are. I'd hate to have that stuff come apart
> > during use. Perhaps it is not likely, but with things like
> > power hammers I don't like taking anything for granted. I
> > have had the upper dies come flying out of a small 25# hammer
> > on two occasions very suddenly. It's not what I'd call a
> > great thrill. YMMV
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>